Laguna Clay

Clay body · by Laguna Clay

Moroccan Sand

Product code WC400 · Fires to cone 5

Published specs

As published by Laguna Clay. Shrinkage is total (wet to fired); absorption is water absorption of the fired body — the closer to 0%, the more vitrified.

ConeShrinkageAbsorption
cone 512%1%
Cone range
cone 5
COE
6.61
Wet colour
Light Brown
Grog
None listed
Maker-suggested uses
Floor Tile, Hand Building Medium, Hand Building Small, Jewelry, Ovenware, Tableware, Throwing Medium, Wall Tile

What the numbers mean at the wheel

Throwing size

At 12% total shrinkage, a form that must finish at 10 cm is thrown at 11.36 cm; a 4-inch mug is thrown at about 4.55 in. Half an inch of the pot disappears in the kiln.

How vitrified

1% absorption at cone 5. Below about 1% is fully vitrified stoneware or porcelain; 1–3% is typical functional stoneware; earthenware sits well above.

Clay for a batch

Fifty 450 g mugs with 10% trim waste need about 24.8 kg (55 lb) of clay — 2 boxes of 50 lb. Same for any body; what changes is how much of each mug ends up on the shelf.

Comparable bodies

Bodies in the same firing range with the closest published shrinkage and absorption — starting points for a substitute, never a drop-in. Test.

BodyMakerConeShrink.Absorp.
Scott's Red214Standard Ceramiccone 612%1%
Umbria266Standard Ceramiccone 4 – 512.5%1%
Porcelain213Standard Ceramiccone 612%2%
Half & HalfWC402Laguna Claycone 512%0.5%
Rsmc Special -6WC429Laguna Claycone 512%0.5%
Gray Stoneware201Standard Ceramiccone 4 – 612%2.5%

Questions

How much does Moroccan Sand shrink?
Laguna Clay publishes 12% total shrinkage at cone 5 — so a form that must finish at 10 cm is thrown at about 11.36 cm. Batches vary; measure a test tile from your own bag before committing a production run.
What cone does Moroccan Sand fire to?
Laguna Clay rates it at cone 5. Fired above its range a body can slump or bloat; fired below it, it stays porous and glaze fit is unpredictable.
Is Moroccan Sand food safe?
Food safety is a property of the fired glaze and the fit between glaze and body, not of the clay alone. A well-vitrified body (low absorption) with a stable, tested glaze is the usual functional combination; test your own.

Working with clay generates respirable silica dust. Wet-clean, ventilate, and wear a NIOSH-approved respirator for dry work; read the manufacturer's SDS for this body.

This information is provided for planning purposes and is derived from publicly available sources including OSHA regulations, NIOSH guidance, and manufacturer safety data sheets. It does not constitute professional safety advice. Consult your material suppliers' SDS documents and applicable local regulations for authoritative safety guidance.

Sources. Specs are the manufacturer's published values, read from the product page on 2026-08-17; nothing else on that page is reproduced. Throwing sizes and batch weights are computed by Claybench with the same formulas as our free shrinkage and clay weight calculators.

Claybench keeps this body's shrinkage on every form you plan

Add a clay body once; throwing sizes, drying times and clay-per-batch follow it through the studio.